型号: SL-DSC610

DSC范围: 0~±600mW

DSC分辨率: 0.01mW

温度分辨率: 0.01℃

温度范围: RT-500°C

升温速率: 0.1~100℃/min

标准: GB/T 19466.2、GB/T 19466.3、GB/T 19466.6、ISO 11357-2、ISO 11357-3、ISO 11357-6

差示扫描量热仪(DSC)专为管道和聚合物的熔点、结晶度和OIT测试而设计。符合ASTM E967和ISO 11357标准,精度为0.1C。现货并准备发货。
发送询盘
产品详情 —差示扫描量热法

应用:管厂出厂检验、科研、生产研发、教学培训、第三方检测中心

Differential Scanning Calorimetry 差示扫描量热仪.jpg


常见问题解答–差示扫描量热仪(DSC)


问:差示扫描量热仪(DSC)的主要用途是什么?

答:DSC 用于测量样品与参比物之间随温度变化的熱流差。它可以检测玻璃化转变(Tg)、熔融、结晶、固化

及氧化等热事件——是高分子与塑料材料鉴别、质量控制及研发中不可或缺的工具。

问:塑料 DSC 测试应遵循哪些标准?

答:ISO 11357 是塑料 DSC 测试的主要标准系列,涵盖总则(第 1 部分)、玻璃化转变温度(第 2 部分)、熔融

与结晶温度(第 3 部分)以及氧化诱导时间(第 6 部分)。ASTM E967 和 E968 分别涉及 DSC 温度校准与热焓校准。

对于管材材料,ISO 11357-6(OIT)尤其相关。

问:什么是 OIT?为什么对管材材料如此重要?

答:OIT(氧化诱导时间)用于测量材料在指定温度下抵抗氧化降解的时间。对于用于热水及燃气输送的 PE、PP 管材,

OIT 是强制性质量指标——它直接反映材料的长期稳定性及抗氧剂体系的效能。产品标准(如 ISO 15876 和 ISO 22391)

通常规定最低 OIT 限值。

问:DSC 可以测试哪些形态的样品?

答:DSC 可测试固体、薄膜、粉末。对于塑料,通常从粒料、管材断面或板材上切取薄片(3–10 mg)。样品需与样品皿

底部保持良好的热接触——平整薄片或细小切块效果最佳。

问:塑料测试需要多宽的温度范围?

答:大多数热塑性塑料的测试在 -50°C 至 350°C 之间。对于 PE 和 PP,-50°C 至 300°C 可覆盖 Tg、熔融及 OIT。对于

PEEK、PPS 等高温工程塑料,可能需要最高 450°C。如果您测试的管材有 OIT 要求,请确保 DSC 支持在 200–220°C 进行恒温保持。

问:每个测试需要多少样品量?

答:通常为 3–10 mg。样品量越小,加热越均匀,峰形越尖锐;但过少的样品会降低信号强度。对于管材的 OIT 测试,

根据 ISO 11357-6,标准样品量为 5–10 mg。

问:需要做哪些校准?

答:温度校准使用已知熔点的标准物质(铟、锡、铅、锌)。热焓校准使用铟的已知熔融热(28.45 J/g)。校准应在与测试相同

的升温速率下进行。建议每 6 个月或在更改温度范围后重新校准。

交货时间证书自定义选项最小起订量
15个工作日内CE否1台

DSC 新品发布 New Product Release — DSC with a Reversible Screen.jpg

National Institute of Metrology


产品询价

We use cookie to improve your online experience. By continuing to browse this website, you agree to our use of cookie.

Cookies

Please read our Terms and Conditions and this Policy before accessing or using our Services. If you cannot agree with this Policy or the Terms and Conditions, please do not access or use our Services. If you are located in a jurisdiction outside the European Economic Area, by using our Services, you accept the Terms and Conditions and accept our privacy practices described in this Policy.
We may modify this Policy at any time, without prior notice, and changes may apply to any Personal Information we already hold about you, as well as any new Personal Information collected after the Policy is modified. If we make changes, we will notify you by revising the date at the top of this Policy. We will provide you with advanced notice if we make any material changes to how we collect, use or disclose your Personal Information that impact your rights under this Policy. If you are located in a jurisdiction other than the European Economic Area, the United Kingdom or Switzerland (collectively “European Countries”), your continued access or use of our Services after receiving the notice of changes, constitutes your acknowledgement that you accept the updated Policy. In addition, we may provide you with real time disclosures or additional information about the Personal Information handling practices of specific parts of our Services. Such notices may supplement this Policy or provide you with additional choices about how we process your Personal Information.


Cookies

Cookies are small text files stored on your device when you access most Websites on the internet or open certain emails. Among other things, Cookies allow a Website to recognize your device and remember if you've been to the Website before. Examples of information collected by Cookies include your browser type and the address of the Website from which you arrived at our Website as well as IP address and clickstream behavior (that is the pages you view and the links you click).We use the term cookie to refer to Cookies and technologies that perform a similar function to Cookies (e.g., tags, pixels, web beacons, etc.). Cookies can be read by the originating Website on each subsequent visit and by any other Website that recognizes the cookie. The Website uses Cookies in order to make the Website easier to use, to support a better user experience, including the provision of information and functionality to you, as well as to provide us with information about how the Website is used so that we can make sure it is as up to date, relevant, and error free as we can. Cookies on the Website We use Cookies to personalize your experience when you visit the Site, uniquely identify your computer for security purposes, and enable us and our third-party service providers to serve ads on our behalf across the internet.

We classify Cookies in the following categories:
 ●  Strictly Necessary Cookies
 ●  Performance Cookies
 ●  Functional Cookies
 ●  Targeting Cookies


Cookie List
A cookie is a small piece of data (text file) that a website – when visited by a user – asks your browser to store on your device in order to remember information about you, such as your language preference or login information. Those cookies are set by us and called first-party cookies. We also use third-party cookies – which are cookies from a domain different than the domain of the website you are visiting – for our advertising and marketing efforts. More specifically, we use cookies and other tracking technologies for the following purposes:

Strictly Necessary Cookies
These cookies are necessary for the website to function and cannot be switched off in our systems. They are usually only set in response to actions made by you which amount to a request for services, such as setting your privacy preferences, logging in or filling in forms. You can set your browser to block or alert you about these cookies, but some parts of the site will not then work. These cookies do not store any personally identifiable information.

Functional Cookies
These cookies enable the website to provide enhanced functionality and personalisation. They may be set by us or by third party providers whose services we have added to our pages. If you do not allow these cookies then some or all of these services may not function properly.

Performance Cookies
These cookies allow us to count visits and traffic sources so we can measure and improve the performance of our site. They help us to know which pages are the most and least popular and see how visitors move around the site. All information these cookies collect is aggregated and therefore anonymous. If you do not allow these cookies we will not know when you have visited our site, and will not be able to monitor its performance.

Targeting Cookies
These cookies may be set through our site by our advertising partners. They may be used by those companies to build a profile of your interests and show you relevant adverts on other sites. They do not store directly personal information, but are based on uniquely identifying your browser and internet device. If you do not allow these cookies, you will experience less targeted advertising.

How To Turn Off Cookies
You can choose to restrict or block Cookies through your browser settings at any time. Please note that certain Cookies may be set as soon as you visit the Website, but you can remove them using your browser settings. However, please be aware that restricting or blocking Cookies set on the Website may impact the functionality or performance of the Website or prevent you from using certain services provided through the Website. It will also affect our ability to update the Website to cater for user preferences and improve performance. Cookies within Mobile Applications

We only use Strictly Necessary Cookies on our mobile applications. These Cookies are critical to the functionality of our applications, so if you block or delete these Cookies you may not be able to use the application. These Cookies are not shared with any other application on your mobile device. We never use the Cookies from the mobile application to store personal information about you.

If you have questions or concerns regarding any information in this Privacy Policy, please contact us by email at . You can also contact us via our customer service at our Site.